The hot grind schedule of work roll in hot strip mills includes the cooling time waiting for grinding after rolling and corresponding compensatory contour.
热磨制度包括工作辊的下机待磨冷却时间及相应的磨削补偿辊形;在分析了整个轧制过程中和轧制结束后工作辊的温度场和热辊形的变化规律的基础上,建立了热带钢轧机工作辊的热磨制度,认为工作辊的下机最佳冷却时间约为2h,其补偿辊形视磨削后待上机时间而定。
The hot grind schedule of work roll in finishing trains of hot rolling is one of the difficult problems that harasses production all the while and is anxious to be solved.
热轧精轧机组工作辊热磨制度是长期困扰热轧生产并急于解决的难题。
Study on the Optimization of Manufacturing Process and the Structure for Superfine Cu-Zn Powder Made by the Methods of Thermal Atomization and Wet Grind;
热喷球磨法制备超细铜锌粉的工艺优化及其组织研究
Preparation of Cu-Zn Ultrafine Powders by the Method of Thermal Spray and Ball Milling & Study on Dispersing of the Powders;
热喷涂球磨法制备超细铜锌粉及其分散性研究
The instruction of the improvement of the grinder for the super hard ball of valve and the principle& the method for the grind.
介绍了球阀的超硬喷涂球体研磨装置的改进及研磨原理和方法。
DISCUSSION ON THE PREPARATION OF THE FORMING MATERIALS OF ABRASIVE WHEEL WITH WEAR-RESISTANT STEEL BALL BY SPRAY GRANULATION
喷雾造粒法制备磨钢球砂轮成形料的探讨
Three methods are adopted to prepare the toner including ball milling,spray drying and pneumatic jet milling.
试验了三种制备墨粉的方法,即球磨机球磨破碎法、喷雾干燥法和气流粉碎机粉碎法;
One Method of Solving Boiler Water wall Tubes High Temperture Gorrosion & Erosion
解决锅炉水冷壁管高温腐蚀和磨损方法之热喷涂技术
abrasion resistance assessment by jet test
喷射试验法评定耐磨性
Preparation of SiC_p/Cu Nanostructure Composite by Ball Milling and Hot Pressed Sintering;
球磨—热压烧结法制备SiC_p/Cu纳米复合材料
A nitrogen heat treatment method of nozzles was proposed for the sharp wear, evident high temperature creep deformation of the nozzles for sulfur atomization.
针对硫磺雾化喷嘴存在磨蚀快、温蠕变明显的现象,提出了喷嘴氮化热处理的方法。
Investigtion of Thermal Spraying Technology for Friction and Wear
热喷涂技术在摩擦磨损领域应用研究
Study on Thermal Sprayed Coating With High-temperature Oxidation Resistance and Wear Resistance
热喷涂高温抗氧化耐磨损涂层的研究
floating suspension nozzle method
喷嘴式热风悬浮烘燥法
Study on the Performance of Wear and Impact of Al_2O_3 Ceramic Thermal Spraying Coating;
Al_2O_3陶瓷热喷涂涂层磨损及冲击性能研究
Microstructure and Properties of Heat- and Wear-resistant Al-Si Alloy Prepared by Spray Deposition;
喷射沉积Al-Si系耐热耐磨合金的组织及性能
Microstructures and Properties of Aluminum Alloy with Heat- and Wear-Resistance Prepared by Spray Forming;
喷射沉积耐热耐磨铝合金的组织和性能研究
The Improvement of M-48 Import Defibrator Blow Valve Hydraulic System
对M-48型进口热磨机喷放阀液压系统的改进
Abrasive resistance of sprayed Al_2O_3-TiO_2 and WC-Co coatings on high temperature ball valve
高温球阀喷涂Al_2O_3-TiO_2和WC-Co涂层的耐磨粒磨损性能
testing method for wear resistance of high performance ceramics by ball-on-disk method
工程陶瓷制品耐磨性试验-磨球盘法